*[http://www.houseofkolor.com/PDF/TechData/English/KP21.pdf House of Kolor Kwikure Epoxy Primer Surfacer tech sheet]:
 
*[http://www.houseofkolor.com/PDF/TechData/English/KP21.pdf House of Kolor Kwikure Epoxy Primer Surfacer tech sheet]:
 
<blockquote>
 
<blockquote>
''"If you find it necessary to use a metal conditioner to remove rust, etc., be sure to thoroughly clean and nutralize the treated area following the conditioner manufacturers recommendations, then using our KC20 post sanding cleaner with a maroon scuff pad to insure all acid residue has been removed before priming. If not, this will almost certainly cause an adhesion problem."''
+
''"'''NOTE:''' Do not use any acid base products such as self etching primer, etc. under the KP2CF primer. This will almost certainly cause an adhesion problem.''
 +
<br>
 +
'''''NOTE:''' If you find it necessary to use a metal conditioner to remove rust, etc., be sure to thoroughly clean and neutralize the treated area following the conditioner manufacturers recommendations, then using our KC20 post sanding cleaner with a maroon scuff pad to insure all acid residue has been removed before priming. If not, this will almost certainly cause an adhesion problem."''
 