Rust, pitted
 (→Handling rust pinholes)  | 
		|||
| Line 37: | Line 37: | ||
*Clamp a piece of copper to the other side of the panel, covering the pinhole. Then, fill the hole in with a MIG welder. When done, unclamp the copper -- it won't stick to the panel, and will act as a heat sink, so the panel doesn't warp as much.  | *Clamp a piece of copper to the other side of the panel, covering the pinhole. Then, fill the hole in with a MIG welder. When done, unclamp the copper -- it won't stick to the panel, and will act as a heat sink, so the panel doesn't warp as much.  | ||
*Drilling and patching -- explain.  | *Drilling and patching -- explain.  | ||
| + | *Solder Flowing can be done with specially formulated flux and solder combinations at temperatures as low as 350 degrees Fahrenheit.  | ||